Skip to main content

Table 4 Number of necessary grains (Confidence value: 95%).

From: Cyclic Biaxial Stress Measurement Method Using the Grain Growth Direction in Electrodeposited Copper Foil

0.16

0.33

0.52

0.72

1.0

[%]

3

330

182

71

48

44

 

5

117

66

26

18

16

 

7

61

34

13

9

8